Advisory Panel
-
-
10-23-2015 09:27 PM
# ADS
Friends and Sponsors
-
Legacy Member
I am a big fan of West System epoxies for cycling and marine use, but the heat deformation temperature (NOT failure point) is only about 120 degrees while the ultimate glass transition temperature is only 120-140 degrees (F)! I know most of us don't really plan on rapid firing our rifles as much as envisioned originally but a handguard must get hotter than that...
So maybe I'll concur that wood glue is for wood.
Last edited by AD-4NA; 10-28-2015 at 01:39 AM.
-
Thank You to AD-4NA For This Useful Post:
-