    Any abrasive method -steel wool or whatever, even a cloth with a cleaning agent - is going to increase wear on edges, corners and the most exposed surfaces, while totally failing to reach right into recesses.
    That is why using the electrolysis method is IMOH the best way to preserve the steel and any remaining bluing.

    And since the electrolytic bath basically has the same effect as the expensive "degreasers/conditioners" sold for cold bluing, you can take a piece out of the electrolytic bath, brush off any loose particles with a stiff brush, flush in clean water, and dunk straight into the bluing bath. On rusted screws, for instance, electrolysis is an excellent way to clean up the threads. Try it on an old blued part or a rusted screw!

  2. # ADS
    Friends and Sponsors
    Join Date
    October 2006
    Location
    Milsurps.Com
    Posts
    All Threads
    A Collector's View - The SMLE Short Magazine Lee Enfield 1903-1989. It is 300 8.5x11 inch pages with 1,000+ photo’s, most in color, and each book is serial-numbered.  Covering the SMLE from 1903 to the end of production in India in 1989 it looks at how each model differs and manufacturer differences from a collecting point of view along with the major accessories that could be attached to the rifle. For the record this is not a moneymaker, I hope just to break even, eventually, at $80/book plus shipping.  In the USA shipping is $5.00 for media mail.  I will accept PayPal, Zelle, MO and good old checks (and cash if you want to stop by for a tour!).  CLICK BANNER to send me a PM for International pricing and shipping. Manufacturer of various vintage rifle scopes for the 1903 such as our M73G4 (reproduction of the Weaver 330C) and Malcolm 8X Gen II (Unertl reproduction). Several of our scopes are used in the CMP Vintage Sniper competition on top of 1903 rifles. Brian Dick ... BDL Ltd. - Specializing in British and Commonwealth weapons Specializing in premium ammunition and reloading components. Your source for the finest in High Power Competition Gear. Here at T-bones Shipwrighting we specialise in vintage service rifle: re-barrelling, bedding, repairs, modifications and accurizing. We also provide importation services for firearms, parts and weapons, for both private or commercial businesses.
     

  3. #12
    Advisory Panel
    Roger Payne's Avatar
    Join Date
    Mar 2008
    Last On
    04-27-2024 @ 05:16 AM
    Location
    Sutton Coldfield, UK.
    Posts
    3,440
    Real Name
    Roger Payne
    Local Date
    05-01-2024
    Local Time
    12:45 AM
    I would endorse what No4 Mk1 T & Patrick say. Many years ago a fellow forummer sent me a scientific paper from an archaeology journal relating how to go about using the electrolytic method & I have been successfully using it for about ten years on recovered WW1 battlefield artefacts as well as small enfield parts. I use an old car battery charger set to trickle charge & a bucket filled with cold water to which I add just a sprinkling of caustic soda (NaOH - sold as crystals in the UKicon for unblocking your drains). Essentially you use the item you want to clean up as your cathode or negative electrode. The anode or positive electrode is sacrificial, (in other words the electrolytic process gradually corrodes it away), so I use clean pieces of scrap steel & replace them or clean them regularly as they get covered in rusty deposit quite quickly & this slows up the electrolytic process. Care must be taken as the caustic soda mix is very strongly alkaline, but in practice you only need a very dilute solution, & so long as you wash any skin splashes immediately with copious water you are not likely to come to much harm.

    The beauty of this method as has already been mentioned is that it eradicates the rust from everywhere & uses no abrasion, so causes no damage whatsoever to the native steel. Incidentally it also works on non-ferrous metals & over the years I have cleaned up hundreds if not into the low thousands of WW1 battlefield recovery cartridge cases in this way.

    ATB
    Last edited by Roger Payne; 03-27-2013 at 07:20 AM. Reason: typo

  4. Avoid Ads - Become a Contributing Member - Click HERE
  5. #13
    Legacy Member tower06's Avatar
    Join Date
    Mar 2009
    Last On
    04-16-2024 @ 09:26 AM
    Location
    New Jersey
    Age
    49
    Posts
    202
    Real Name
    Mariusz Strus
    Local Date
    04-30-2024
    Local Time
    07:45 PM
    Thread Starter
    I will have to give it a shot. Thanks again gents.

  6. #14
    Legacy Member Roy's Avatar
    Join Date
    Mar 2009
    Last On
    04-22-2023 @ 04:09 AM
    Location
    NZ/Ocean
    Posts
    352
    Real Name
    Roy
    Local Date
    04-30-2024
    Local Time
    07:45 PM
    With inspiration from this tread I built a de-rusting bath, and it works great. Though the battery charger had some sort of safety that meant it didnt work when not charging a battery. I've used a old mobile phone charger and some resistors to alter the current. There are some good instructions on the net on how to build them too. Got to go and check on a SMLE nosecap now.
    Keep Calm
    and
    Fix Bayonets

  7. Thank You to Roy For This Useful Post:


  8. #15
    Legacy Member frankderrico's Avatar
    Join Date
    Mar 2009
    Last On
    Today @ 03:30 PM
    Location
    Central Wisconsin
    Posts
    1,629
    Real Name
    Frank Derrico
    Local Date
    04-30-2024
    Local Time
    06:45 PM
    I made one to out of 4" heavy plastic pipe with elbows on the ends. I cut out a chanel and mounted it in a 2X4 cradle. I used a battery charger. About four hours. I needed to derust a half octagon half round fowler, it worked great. When done not much finish but the rust is gone inside and out. It looks alot better and I think it is going to be able to shoot when done.....Frank

  9. Thank You to frankderrico For This Useful Post:


  10. #16
    Legacy Member tower06's Avatar
    Join Date
    Mar 2009
    Last On
    04-16-2024 @ 09:26 AM
    Location
    New Jersey
    Age
    49
    Posts
    202
    Real Name
    Mariusz Strus
    Local Date
    04-30-2024
    Local Time
    07:45 PM
    Thread Starter
    Quote Originally Posted by frankderrico View Post
    I made one to out of 4" heavy plastic pipe with elbows on the ends. I cut out a chanel and mounted it in a 2X4 cradle. I used a battery charger. About four hours. I needed to derust a half octagon half round fowler, it worked great. When done not much finish but the rust is gone inside and out. It looks alot better and I think it is going to be able to shoot when done.....Frank
    I thought the electrolytic bath maintains the finish?

  11. #17
    Advisory Panel Patrick Chadwick's Avatar
    Join Date
    Sep 2008
    Last On
    06-25-2023 @ 06:36 AM
    Location
    Germany
    Posts
    5,032
    Local Date
    05-01-2024
    Local Time
    01:45 AM
    Quote Originally Posted by Roy View Post
    Though the battery charger had some sort of safety that meant it didnt work when not charging a battery.

    That may be a device that switches it off if the current falls below a minimum level, to prevent overcharging. The answer is to provide that minimum load by wiring a suitable resistance in parallel with the bath. Something that will draw about 50 mA should be enough.

  12. #18
    Advisory Panel
    Roger Payne's Avatar
    Join Date
    Mar 2008
    Last On
    04-27-2024 @ 05:16 AM
    Location
    Sutton Coldfield, UK.
    Posts
    3,440
    Real Name
    Roger Payne
    Local Date
    05-01-2024
    Local Time
    12:45 AM
    Tower, the original finish should be maintained, but I just wondered if frankderrico's old fowler was rather more patinated than blued?? If so, the patination (being low grade corrosion) would come off.

    ATB
    Last edited by Roger Payne; 04-18-2013 at 06:02 PM.

  13. #19
    Legacy Member blackcat_attilio's Avatar
    Join Date
    Dec 2009
    Last On
    10-01-2020 @ 04:27 PM
    Location
    Northern Italy
    Age
    64
    Posts
    134
    Local Date
    05-01-2024
    Local Time
    01:45 AM
    Thanks to all you for so many suggestions. Useful.

    Blackcat

  14. #20
    FREE MEMBER
    NO Posting or PM's Allowed
    CrossedCannons's Avatar
    Join Date
    Jan 2010
    Last On
    08-20-2017 @ 08:56 AM
    Location
    Horse country, AZ
    Posts
    351
    Local Date
    04-30-2024
    Local Time
    04:45 PM
    "Blueing" is a form of oxidized iron (Fe3O4), just not the more highly oxidized "red" form (Fe2O3). Electrolysis reduces oxidized iron to metallic iron. So while I've never attempted to "derust" a blued part, I would be very very surprized if any "bluing" remains after "the bath"

+ Reply to Thread
Page 2 of 3 FirstFirst 1 2 3 LastLast

Similar Threads

  1. To do or not to do (removing rust)?
    By MeatMarket in forum Edged Weapons Forum
    Replies: 26
    Last Post: 01-06-2012, 10:32 PM
  2. Moving Forward: Rust
    By Wolf308 in forum The Lee Enfield Knowledge Library Collectors Forum
    Replies: 3
    Last Post: 09-26-2011, 09:58 AM
  3. Bore rust/corrosion removal?
    By ANDYZ28 in forum The Lee Enfield Knowledge Library Collectors Forum
    Replies: 9
    Last Post: 07-16-2011, 05:17 AM
  4. BR rust/pitting problems
    By AFS in forum M1 Garand/M14/M1A Rifles
    Replies: 4
    Last Post: 05-26-2009, 09:45 PM
  5. Rust Bluing Problem
    By Jim Tarleton in forum Gunsmithing for Old Milsurps
    Replies: 4
    Last Post: 05-22-2009, 01:52 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts